| Wood questionsMay 27 2008 at 9:35 AM | Jim Thompson |
| Hi Gang,
I have two questions.
1. How long do you need to allow CPES to dry/cure before placing two boards together with a caulk/sealent e.g. 5200 ?
2. I have heard that you should add salt to the water, to raise the boiling temperature, when steaming wood. This weekend I heard that amonia should be added to the water. What affects does the amonia have on the water or wood?
Thanks,
Jim (Fiberglass) Thompson
p.s. Yes, I am playing with a wood boat. |
| | Author | Reply | phil mitchell | Re: Wood questions | May 27 2008, 9:59 PM |
CPES is manufactured by Smith and Compamy www.smithandcompany.org. Call them at 1-[Telephone number archived] or 1-[Telephone number archived]. They can give you better advice than anyone here can.
As to the salt/ammonia, if you do, you're inducing minute amounts of sodium chloride and or ammonia into the wood. Are you sure you want to do that? I'd check with someone that builds boats with steam bent parts. Or, contact Travis Hickman at Hickman Boat Works. He might be able to shed some light on it for you.
Phil |
| Harris | Smiths | May 27 2008, 10:17 PM |
Jim, I've used Smiths on everything from the boat to bird houses. Follow the instructions, don't let it puddle up and wipe up all that does. You put down only what will soke in. You'll know when its dry, its pretty obvious. It should take no more than over night. If its takey after that, I'd say you put on too much. Good luck. |
| | | | |
|
|
|